Figure 9. Defective bonding. SEM micrograph of a specimen that was overdried after the etching gel was rinsed off. In such cases, the adhesive resin cannot penetrate the demineralized dentin because of the collapse of the collagen network (arrows) (orig. mag. x 10,000).